内容简介Materials B and C were used in the waste melting furnace. In the case of conventional material A, tortoise shell-like cracks developed in two months and then partially fell down after three months. Material B has been used for three months, showing good performance without cracking. Material C has also been used for five months, showing good performance without the tortoise shell-like cracks, but with some peeling by pushing-out. It is considered that Material C can be effectively used in locations where corrosion resistance is required.