内容简介Formulations for deflocculated or self-flow castables rely on the use of fine, reactive matrix fillers to optimise the packing density in the cast mass. At the same time, it is possible to reduce the calcium aluminate cement (CAC) content due to the higher inter-granular contact of the system. When ultra fine fillers are dispersed in water, a surface charge appears due to the -OH groups formation and proton exchange. In order to decrease the surface energy, fine particles tend to agglomerate in water and this creates flocculation. It is thus necessary to add dispersing/fluidifying additives to disperse the system.